TP037 – The Development of Very High Strength Copper Nickel alloys with Resistance to Hydrogen Embrittlement and Stress Corrosion Cracking

TP037 – The Development of Very High Strength Copper Nickel alloys with Resistance to Hydrogen Embrittlement and Stress Corrosion Cracking

Descrizione:

This paper reviews the use of slow strain rate testing as a suitable measure of high-strength copper alloys where hydrogen embrittlement might be a concern. The development of Hiduron 220 is considered against these test results.

 

Project Overview:

  • Market Sector: Marine
  • Authors: C. Tuck
  • Company: Langley Alloys
  • Publication Date: 2005